Synthesis and characterization study of n-Bi2O3/p-Si heterojunction dependence on thickness
...Show More Authors
Ethanol as a solvent, a precursor of titanium isopropoxide and a stabilizer of either hydrochloric acid or ammonium hydroxide was used to prepare a titanium dioxide aqueous solution. The aqueous solutions with different values of pH and the morphology of the resultant reaction of the nanoparticles of titanium dioxide were investigated. The X-ray diffraction showed that at low temperatures and with acidic solutions, rutile structures are more favorable to grow on titanium dioxide synthesized, while at low and average temperatures and with base solutions, anatase phase is more pronounced. The crystalline form and the re-confirmation of the crystallite size growth were observed by the scanning electron microscopy. The atomic force micr
... Show MoreBackground & objective: Difficult intubation remains a risk for patients undergoing general anesthesia (GA) or mechanical ventilation in an intensive care unit (ICU). Macroglossia is a known factor for difficult intubation. But it is not routine to assess the tongue size to predict difficult intubation. Studies are found deficient in comparing usefulness of measuring thyromental distance and the tongue thickness (TT) measured by ultrasonography to estimate difficult intubation. We compared tongue thickness measured by ultrasonography and thyromental distance as a means to anticipate difficult intubation. Methodology: A convenient sample of 60 patients; 32 males and 28 females, who were undergoing elective surgery with GA were i
... Show MoreTwo simple methods for the determination of eugenol were developed. The first depends on the oxidative coupling of eugenol with p-amino-N,N-dimethylaniline (PADA) in the presence of K3[Fe(CN)6]. A linear regression calibration plot for eugenol was constructed at 600 nm, within a concentration range of 0.25-2.50 μg.mL–1 and a correlation coefficient (r) value of 0.9988. The limits of detection (LOD) and quantitation (LOQ) were 0.086 and 0.284 μg.mL–1, respectively. The second method is based on the dispersive liquid-liquid microextraction of the derivatized oxidative coupling product of eugenol with PADA. Under the optimized extraction procedure, the extracted colored product was determined spectrophotometrically at 618 nm. A l
... Show MoreSchiff base obtained from the reaction (Trimethoprim) with (sodiumpyruvate ) to produce the ligand [NaL], the reaction was carried out in methanol as a solvent under reflux. The prepared ligand [NaL] was characterized by FT-IR, UV-Vis spectroscopy, 1H,13C-NMR spectra, mass spectra, and melting point.A new mixed ligand complexes have been prepared between ( 8- hydroxyquinolone) and the ligand [NaL] withMn(II).Co(II),Ni(II),Cu(II), (Zn(II) ,(Cd(II)and Pd(II). All the complexes were characterized by spectroscopic methods (FT-IR, UV-Vis spectroscopy), chloride content and melting point ,molar conductance and magnetic susceptibility.These measure- ments showed octahedral geometry around(,Mn2+, Co2+, Ni2+, Cu2+, Zn2+ and Cd2+) ions and square pla
... Show MoreAbstract. Silver, Indium Selenium thin film with a thickness (5001±30) nm, deposited by thermal evaporation methods at RT and annealing3temperature (Ta=400, 500 and 600) K on a substrate of glass to study structural and optical properties of thin films and on p-Si wafer to fabricate the AgInSe2/p-Si heterojunction solar cell. XRD analysis shows that the AgInSe2 (AIS) deposited film at RT and annealing3temperature (Ta=400, 500 and 600) K have polycrystalline structure. The average grain size has been estimated from AFM images. The energy gap was estimated from the optical transmittance using a spectrometer type (UV.-Visible 1800 spectra photometer). From I-V characterization , the photovoltaic parameters such as, open-circuit voltage, short
... Show MoreMeasurements of Hall effect properties at different of annealing temperature have been made on polycrystalline Pb0.55S0.45 films were prepared at room temperature by thermal evaporation technique under high vacuum 4*10-5 torr . The thickness of the film was 2?m .The carrier concentration (n) was observed to decrease with increasing the annealing temperature. The Hall measurements showed that the charge carriers are electrons (i.e n-type conduction). From the observed dependence on the temperature, it is found that the Hall mobility (µH), drift velocity ( d) carrier life time ( ), mean free path (?) were increased with increasing annealing temperature