ABSTRACT Background: resin cement type and intraoral temperature fluctuations may affect the fracture performance of successful zirconia restorations. To fill this gap, the purpose of this study is to evaluate and compare the influence of thermocycling on fracture resistance and mode of failure of monolithic zirconia crowns luted with Rely X™ U200 and BreezeTMself-adhesive resin cements as well as imply the effect of adding 2 % of polylysine (PLS) to these cements. Materials: 64 maxillary premolars were milled out of zirconia blocks using CAD/CAM milling system. They were divided into four groups (n = 16) according to the cement type. Four different resin cements were used (RelyXTMU200, Breeze™, RelyX™ U200 with 2 % PLS and Breeze™ with 2%PLS). Each group was further subdivided into experimental and control groups (n = 8). The experimental specimens were exposed to thermocycling protocol of 10,000 cycles in water bath at 5 ◦C and 55 ◦C.Each specimen was subjected to axial load until fracture using universal testing machine. Fracture modes were analyzed using digital microscope. Data were statistically analyzed using paired t-test at a level of significance of 0.05. Results: there was a statistical significant difference in fracture load among groups (p < 0.05) with the highest mean in Rely X cement. Although the fracture loads statistically decreased after thermocycling (p < 0.05) there was no significant effect on the addition of 2 % PLS (p > 0.05). Microscopical analysis demonstrated a majority of catastrophic mode of fracture. Conclusion: both cement type and thermocycling exert significant effects on fracture resistance of premolars crowns restored with monolithic zirconia, while the addition of 2 % PLS exerted negligible effec
It is found that hypersensitive teeth have a larger number and wider patent tubules than those of non-sensitive teeth. Objective: The aim of this study is to compare between the effects of diode laser at different power densities, with and without sodium fluoride on the sealing of exposed dentinal tubules and dentin permeability. Materials and methods: 118 teeth were used. Samples were divided into three major groups. The first consisted of 100 teeth used for permeability test. The second consisted of 16 teeth for measuring external surface temperature elevation while irradiation. The third, in turn, consisted of one pair of teeth observed under SEM for dentine surface morphology analysis. Results: For dentin permeability measurement, th
... Show MoreBackground: The bonded orthodontic retainer constructed from multistrand wire and composite is an efficient esthetic retainer, which can be maintained long-term. Clinical failures of bonded orthodontic retainers, most commonly at the wire/composite interface, have been reported. This in vitro investigation aimed to evaluate the tensile forces of selected multistrand wires and composite materials that are available for use in the construction of bonded fixed retainers. Materials and Methods: The study sample includes 120 wires with three types of retainer wires (3 braided strands\ Orthotechnology, 8 braided strands\ G&H Orthodontics, 6 coaxial strands\ Orthoclassic wires), two types of adhesive (flowable\ Orthotechnology, non flowable\ G&H O
... Show MoreSchiff base derived from PVA and Erythroascorbic acid derivative (pentulosono-ɣ-lactone-2, 3-enedianisoate) was synthesized and characterized by Thin Layer Chromatography (TLC) and FTIR spectra, aldehyde was also characterized by (U.V-Vis), 1HNMR, 13CNMR and mass spectra. The inhibitory effect of prepared polymer on the activity of human serum Cholinesrerase has been studied in vitro. The polymer showed a remarkable activity at low concentration (4.5*10-3 – 4.5*10-8 M).
Background: The aim of this in vitro study was to evaluate and compare the microleakage between Vertise Flow T M composite material and other conventional (Filtek Z250, riva light cure and SDR) composite materials when restoring CII mesial box only cavity at gingival margin through die penetration test Materials and methods: Forty maxillary first premolars were prepared with class II box design only cavities. Samples were divided into four groups of ten teeth according to material used: group I (FiltekZ250 only). Group II (SDR+FiltekZ250). Group III (Vertise Flow +FiltekZ250). Group IV (Riva light cure+ FiltekZ250). After 24 hrs. immersion in 2% in methylene blue, samples were sectioned and micro leakage was estimated. Results: None of the
... Show MoreIntroduction and Aim: Pseudomonas aeruginosa is a nosocomial infection with an ability to develop high levels of antibiotic resistance. The efflux pump system is one of the mechanisms that is linked to multidrug resistance in P. aeruginosa. In this study, we employed siRNA loaded on gold nanoparticles against the MexA efflux pump gene to decrease the MexA gene expression in P. aeruginosa and estimated antibiotic resistance after gene silencing. Materials and Methods: This study examined four strains of P. aeruginosa isolated from patients in various hospitals in Baghdad. Bacteria isolated were identified by biochemical tests and Vitek compact 2 system. Single-stranded siRNA (33bp) designed in this study was loaded onto gold
... Show MoreAbstract
In the present study, composites were prepared by Hand lay-up molding. The composites constituents were epoxy resin as a matrix, 6% volume fractions of glass fibers (G.F) as reinforcement and 3%, 6% volume fractions of preparation natural material (Rice Husk Ash, Carrot Powder, and Sawdust) as filler. Studied the erosion wear behavior and coating by natural wastes (Rice Husk Ash) with epoxy resin after erosion. The results showed the non – reinforced epoxy have lower resistance erosion than natural based material composites and the specimen (Epoxy+6%glass fiber+6%RHA) has higher resistance erosion than composites reinforced with carrot powder and sawdust at 30cm , angle 60
... Show MoreEfficacy of Varnishes with: Bioactive Glass, Recaldent Technology and Silver Diamine Fluoride in Comparison with Sodium Fluoride on Tooth Surface Micro-hardness (an In Vitro Study)
In this search, Ep/SiO2 at (3, 6, 9, 12 %) composites is prepared by hand Lay-up method, to measure the change in the thermal conductivity and Impact Strength of epoxy resin before and after immersion in H2SO4 Solution with a 0.3N for 10 days. The results before immersion decreases with the increase of the weight ratios of the reinforcement material (SiO2), It changed from (82.6×10-2 to 38.7×10-2 W/m.°C) with change weight ratios from (3 to 12) % respectively, but after immersion time in the chemical solution where it was (65.6×10-2 W/m.°C) at the weight ratios (6 %) and became (46.6 × 10-2 W/m.°C) after immersion in sulfuric acid. The results of the Impact strength decreased by increasing the percentage weight ratio, it changed f
... Show More