Abstract Ternary Silver Indium selenide Sulfur AgInSe1.8S0.2 in pure form and with a 0.2 ratio of Sulfur were fabricated via thermal evaporation under vacuum 3*10-6 torr on glasses substrates with a thickness of (550) nm. These films were investigated to understand their structural, optical, and Hall Characteristics. X-ray diffraction analysis was employed to examine the impact of varying Sulfur ratios on the structural properties. The results revealed that the AgInSe1.8S0.2 thin films in their pure form and with a 0.2 Sulfur ratio, both at room temperature and after annealing at 500 K, exhibited a polycrystalline nature with a tetragonal structure and a predominant orientation along the (112) plane, indicating an enhanced degree of crystallinity. The Atomic Force Microscopy (AFM) was utilized to explore how Sulfur affects roughness of surfaces and sampls Grain Size . Furthermore, optical parameters, such as the optical gap and absorption coefficient, were calculated to assess the influence of Sulfur on the optical properties of the AgInSe1.8S0.2 thin films. The UV/Visible measurements indicated a reduction in the energy band gap to 1.78 eV for AgInSe1.8S0.2 at 500 K, making these films potentially suitable for photovoltaic applications. These thin films exhibited donor characteristics, with an increase in electron concentration observed with higher Sulfur content and annealing temperature
The present study focuses on synthesizing solar selective absorber thin films, combining nanostructured, binary transition metal spinel features and a composite oxide of Co and Ni. Single-layered designs of crystalline spinel-type oxides using a facile, easy and relatively cost-effective wet chemical spray pyrolysis method were prepared with a crystalline structure of MxCo3−xO4. The role of the annealing temperature on the solar selective performance of nickel-cobalt oxide thin films (∼725 ± 20 nm thick) was investigated. XRD analysis confirmed the formation of high crystalline quality thin films with a crystallite si
The structural, optical and electrical properties of ZnS films prepared by vacuum evaporation technique on glass substrate at room temperature and treated at different annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction studies show that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (111). The optical properties investigated which include the absorbance and transmittance spectra, energy band gab, absorption coefficient, and other optical constants. The results showed that films have direct optical transition. The optical band gab was found to be in the range t
... Show MoreIn the present work we prepared heterojunction not homogenous CdS/:In/Cu2S) by spray and displacement methods on glass substrate , CdS:In films prepared by different impurities constration. Cu2S prepared by chemical displacement method to improve the junction properties , structural and optical properties of the deposited films was achieved . The study shows that the film polycrystalline by XRD result for all film and the energy gap was direct to 2.38 eV with no effect on this value by impurities at this constration .
M(II) Ions using amino acid L- proline as a primary ligand and either Nicotinamide or 8- hydroxyqinoline as secondary ligand, respectively: a. The mixed ligand complexes of composition,[M(pro)2(na)2]. b. The mixed ligand complexes of composition , Na[M(pro)2(Q)]. Where proline (C5H9NO2) symbolized as pro H , Nicotinamide (C6H6N2O) symbolized as (NA) , 8- hydroxyqinoline, (C9H7NO2) symbolized as (8-HQ). The ligands and the metal chlorides were brought into reaction at room temperature (37ºc) in ethanol as solvent .The reaction required the following molar ratios [(1:2:2) metal:2NA:2pro-] and [(1:1:2) metal:Q:2pro-] with M+2 ions, where M = [Mn (II), Co(II), Ni(II), Cu(II), Zn(II), Cd(II) and pd(II)]. Products were found to be solid crystall
... Show MoreThin films of GexS1-x were fabricated by thermal evaporating under vacuum of 10-5Toor on glass substrate. The effect of increasing of germanium content (x) in sulfide films on the electrical properties like d.c conductivity (σDC), concentration of charge carriers (nH) and the activation energy (Ea) and Hall effect were investigated. The measurements show that (Ea) increases with the increasing of germanium content from 0.1to0.2 while it get to reduces with further addition, while charge carrier density (nH) is found to decrease and increase respectively with germanium content. The results were explained in terms of creating and eliminating of states in the band gap