Wastewater discharge containing organic dyes may pose a hazard to the environment, which necessitates that dye removal must occur prior to wastewater release into water bodies. Herein, copper oxide nanoparticles (CuO NPs) were prepared by a green precipitation method to enable decolorization of a cationic dye (methyl violet; MV) from aqueous media. Complementary tools were employed to characterize the CuO NPs adsorbent: spectroscopy (FTIR and UV-VIS), microscopy (FESEM and TEM), XRD, BET surface area analysis, and point of zero charge (pHPZC) via potentiometry. The FTIR bands at 722, 663, 569, and 465 cm1 correspond to the vibrational modes of CuO NPs, along with the optical absorbance band at 275 nm that supports the formation of CuO NPs. The XRD and TEM analyses predicted single-phase CuO NPs with a monoclinic framework. BET was employed to assess the textural characteristics and accounted for the specific surface area (12.97 m2·g1). Batch adsorption studies were carried out to assess the role of initial pH (3.58–10.53), CuO NPs dose (0.02–0.25 g/L), initial MV concentration (20–140 mg/L), contact time (5–90 min), and temperature (298, 308, and 318 K) on the dye removal efficiency. The adsorption capacity of CuO NPs for MV was determined to be 5.06 mg/g at 45°C. The pseudo-second-order (PSO) model described kinetic isotherms, and equilibrium adsorption data were adequately fitted by the Freundlich model. Thermodynamic results revealed that adsorption was spontaneous, endothermic, and entropy driven at the solid–liquid interface. The CuO NPs further displayed good reusability with high efficiency for six successive cycles of adsorption–desorption using 0.1 M HCl as a desorbing agent. These findings validate the efficacy of CuO NPs as a green and effective adsorbent for wastewater treatment processes for cationic dye removal.
The synthesis oxadiazole derivative 2,5-disubstituted-1,3,4oxadiazole (3a,3b,3c) was prepared from reaction of N-(4-amino benzene sulphonyl)Morpholipebut-2-enehydrazide with (4-hydroxybenzaldehyde,4-methoxy benzaldehyde,4-ethoxybenzaldehyde) in the presence of lone as catalyst. The structure of (3a,3b,3c) was characterized by using FT-IR, H-NMR and spectroscopy. Nanoparticles of the prepared compounds have been fabricated in aqueous media using re-precipitation method.Characterization of the nano particles (ONPs) have been performed by using UV-VIS spectrophotometer and scanning electron micro scope ( SEM). The size of the nanoparticales were around 150-200 nm as indicated by (SEM). T
Graphite nanoparticles were successfully synthesized using mixture of H2O2/NH4OH with three steps of oxidation. The process of oxidations were analysis by XRD and optics microscopic images which shows clear change in particle size of graphite after every steps of oxidation. The method depend on treatments the graphite with H2O2 in two steps than complete the last steps by reacting with H2O2/NH4OH with equal quantities. The process did not reduces the several sheets for graphite but dispersion the aggregates of multi-sheets carbon when removed the Van Der Waals forces through the oxidation process.
In this study, the acid-alkaline transesterification of refined coconut seed oil (RCOSO) to fatty acid methyl ester was followed by the production of a trimethylolpropane-based thermosensitive biolubricant using potassium hydroxide, and its physicochemical characteristics were evaluated. The American Standard Test for Materials (ASTM) was employed to ascertain the biolubricant's pour point and index of viscosity, which were found to be -4 oC and 283.75, respectively. The opposite connection between lubricant viscosity and temperature was shown by the measured viscosities at varied transesterification to be transformed into biodiesel. Following this, a biolubricant was created by further transesterifiedtemperature. The ester gr
... Show MoreThe semiempirical (PM3) and DFT quantum mechanical methods were used to investigate the theoretical degradation of Indigo dye. The chemical reactivity of the Indigo dye was evaluated by comparing the potential energy stability of the mean bonds. Seven transition states were suggested and studied to estimate the actually starting step of the degradation reaction. The bond length and bond angle calculations indicate that the best active site in the Indigo dye molecule is at C10=C11. The most possible transition states are examined for all suggested paths of Indigo dye degradation predicated on zero-point energy and imaginary frequency. The first starting step of the reaction mechanism is proposed. The change in enthalpy, Gibbs free energ
... Show MoreIn this work the fabrication and characterization of poly(3-hexylthiophene) P3HT-metallic nanoparticles (Ag, Al). Pulsed Laser Ablation (PLA) technique was used to synthesis the nanoparticles in liquid. The Fourier Transformer Infrared (FTIR) for all samples indicate the chemical interaction between the polymer and the nanoparticles. Scanning Electron Microscopic (SEM) analysis showed the particle size for P3HT-AgNps samples between 44.50 nanometers as well the spherical structure. While for P3HT-AlNps samples was flakes shape. Energy Dispersive X-ray (EDX) spectra show the existing of amount of metallic nanoparticles.
This work aim to prepare Ag/R6G/PMMA nanocomposite thin
films by In-situ plasma polymerization and study the changes in the
optical properties of fluorophore due to the presence of Ag
nanoparticles structures in the vicinity of the R6G laser dye. The
concentrations of R6G dye/MMA used are: 10-4M solutions were
prepared by dissolving the required quantity of the R6G dye in
MMAMonomer. Then Silver nanoparticles with 50 average particles
size were mixed with MMAmonomer with concentration of 0.3, 0.5,
0.7wt% to get R6G silver/MMA in liquid phase. The films were
deposited on glass substrates by dielectric barrier discharge plasma
jet. The Ag/R6G/PMMA nanocomposite thin films were
characterization by UV-Visible
In this study, gold nanoparticle samples were prepared by the chemical reduction method (seed-growth) with 4 ratios (10, 12, 15 and 18) ml of seed, and the growth was stationary at 40 ml. The optical and structural properties of these samples were studied. The 18 ml seed sample showed the highest absorbance. The X- ray diffraction (XRD) patterns of these samples showed clear peaks at (38.25o, 44.5o, 64.4o, and 77.95o). The UV-visible showed that the absorbance of all the samples was in the same range as the standard AuNPs. The field emission-scanning electron microscope (FE-SEM) showed the shape of AuNPs as nanorods and the particle size between 30-50 nm. Rhodamine-610 (RhB) was prepared at 10<
... Show MoreIn this research, silver nanoparticles (AgNPs) were manufactured using aqueous extract of mushroom Pleurotus ostreatus. Anticancer potential of AgNPs was investigated versus human breast cancer cell line (MCF-7). Cytotoxic response was assessed by MTT assay. AgNPs showed inhibition effect at the following concentrations 12.5, 25, 50, 100 and 200 µg/ml versus MCF-7 cell line, and all treatments had a positive result. The MCF-7 cells were inhibited up to 85.14 % at the concentration 200 μg/ml of AgNPs which reduced cells viability to 14.86%, while 12.5 μg/ml of AgNPs caused 24.23% cells inhibition with reduction of cells viability to 75.77%.