The a.c conductivity and dielectric properties of the prepared composites NiO:ZnO composites samples with various mixing ratios (100:0,80:20,60:40,40:60,20:80 and 0:100) wt. % were carried out . The structure phase, the crystallite size and purity of the fabricated NiO:ZnO composites were confirmed using x-ray diffraction pattern. The results declared that the diffraction spectrum of composites samples were compatible with cubic and hexagonal structures phases for 100%NiOand ZnO respectively while the spectrum were compatible with both phases for the residual composites samples. The crystallite size of the most pronounced plane (101) for crystal growth was changed from 23 nm to 49 .4 nm by increasing of mixing ratio of ZnO from 0 to 100wt%. The dielectric properties were studied as function of frequency in the range (50-50x10 6 Hz). The a.c conductivity σa.c(ω) showed power low dependence for the full frequency range except the composite’s samples 40, 60 %wt. ZnO where there was d.c region in low frequency region range. The exponent (s) values get to change in non-regular sequence as a result of the increasing of ZnO ratio. The real and imaginary dielectric constant ε1 and ε2 were found to increase in non-regular sequence by continuous addition of ZnO to the host oxide. The potential barrier (Wm)for hopping was found to reduce while the density of states at Fermi level N(E f)was found to increase non- systematically by increasing of ZnO ratio. The values of polarizability (α) were calculated and explained.
Nanoparticles of Pb1-xCdxS within the composition of 0≤x≤1 were prepared from the reaction of aqueous solution of cadmium acetate, lead acetate, thiourea, and NaOH by chemical co-precipitation. The prepared samples were characterized by UV-Vis spectroscopy(in the range 300-1100nm) to study the optical properties, AFM and SEM to check the surface morphology(Roughness average and shape) and the particle size. XRD technique was used to determine the crystalline structure, XRD technique was used to determine the purity of the phase and the crystalline structure, The crystalline size average of the nanoparticles have been found to be 20.7, 15.48, 11.9, 11.8, and 13.65 nm for PbS, Pb0.75Cd0.25S,
... Show MoreUsing an environmentally friendly chemical process, a novel nanocomposite consisting of reduced graphene oxide (rGO) and silver(I) oxide (Ag2O) nanoparticles was successfully synthesized in this work, and its optical properties along with photoelectric performance were investigated. Ag2O is a narrow-bandgap p-type semiconductor with strong visible light response but exhibits poor carrier separation and structural instability during exposure to radiation. In order to overcome shortcomings encountered with Ag2O, rGO was used as a conductive support to produce rGO@Ag2O nanocomposites with improved electronic interactions. Various characterization tests, including energy-dispersive X-ray spectroscopy (EDXS), field emission scanning electron mic
... Show MoreIn vivo study revealed that ZnO nanoparticles treatment of Streptococcus SPP contaminated injured skin showed good prognosis and good healing process include complete regeneration of the epithelial cells of the epidermis and increase of cellulartiy of the dermal content compared with untreated group. In conclusion, treatment of S. pyogenes infected skin with Zinc oxide nanoparticles concentration (2 mg/ml) limit the skin damage and localized the lesion to the incision site with good healing process
Polycrystalline ingots of cadmium telluride have been synthesized using the direct
reaction technique, by fusing initial component consisting from pure elements in
stoichiometric ratio inside quartz ampoule is evacuated 10-6 torr cadmium telluride has
been grown under temperature at (1070) oC for (16) hr. was used in this study, the phases
observed in growing CdTe compound depend on the temperature used during the growth
process. Crystallography studies to CdTe compound was determined by X-ray diffraction
technique, which it has zinc blend structure and cubic unit cell, which lattice constants is
a=6.478
oA
Thin films of highly pure (99.999%) Tellurium was prepared by high vacuum technique (5*10-5torr), on glass substrates .Thin films have thickness 0.6m was evaporated by thermal evaporation technique. The film deposited was annealed for one hour in vacuum of (5*10-4torr) at 373 and 423 K. Structural and electrical properties of the films are studies. The x-ray diffraction of the film represents a poly-crystalline nature in room temperature and annealed film but all films having different grain sizes. The d.c. electrical properties have been studied at low and at relatively high temperatures and show that the conductivity decreases with increasing temperature at all range of temperature. Two types of conduction mechanisms were found to d
... Show MoreBaTiO3 thin films have been deposited on Si (111) and glass substrates by using pulsed laser deposition technique. The films were characterized by using X-ray diffraction, atomic force microscope and optical transmission spectra. The films growth on Si after annealing at 873K showed a polycrystalline nature, and exhibited tetragonal structure, while on glass substrate no growth was noticed at that temperature. UV-VIS transmittance measurements showed that the films are highly transparent in the visible wavelength region and near-infrared region for sample annealing on glass substrate. The optical gap of the film were calculated from the curve of absorption coefficient (αhν) 2 vs. hν and was found tobe 3.6 eV at substrate temperature 5
... Show MoreIn this work, the structure properties of nano Lead sulfide PbS thin films are studied. Thin samples were prepared by pulse laser deposition and deposited on glass substrates at wavelength 1064nm wavelength with a various laser energies (200,300,400,500)nm. The study of atomic force microscope (AFM) and X-ray diffraction as well as the effect of changing the laser energy on the structural properties has been studied. It has been observed that the membrane formed is of the polycrystalline type and the predominant phase is the plane (111) and (200). The minimum grain size obtained was 16.5 nm at a laser energy about 200 mJ. The results showed that thin films of average granular sizes (75 nm) could be prepared.As for the optical properties,
... Show More