Objective: The purpose of this work was to develop and optimize the emulgel formulation of piroxicam with two types of gelling agent chitosan and xanthan gum. The release profiles of prepared formulas were investigated. In addition, the rheology and stability of the best formula were investigated.Methods: Emulsified piroxicam was prepared to use oleic acid, tween 80 and PG with a ratio (3:10:10). In xanthan based emulgel, the xanthan gum (1% and 1.5%) was spread as powder on emulsified piroxicam with stirring until emulgel was formed. In chitosan-based emgels, Chitosan gel was added to emulsified piroxicam and stirring until the Emulgel was constructed. Chitosan gels were prepared by incorporating different concentration, 2%, 3%, 6% w/v of chitosan in 1% v/v of glacial acetic acid in distilled water. In vitro release of piroxicam from different formulas was conducted in 300 ml phosphate buffer pH 7.4, at a speed of 120 rpm at 37±2°C. The amount of the drug released from the bases was determined spectrophotometrically at 504 nm. Viscometer Myr. Vr 3000 was used to measure the viscosity of the prepared formulas. The prepared formulas were stored in well-stoppered polyvinyl chloride (PVC) plastic containers in the dark for 6 mo at room temperature. They were checked for drug content, viscosity, and pH change bimonthly throughout the period.Results: The results showed that the dissolution increases significantly with increasing the concentration of xanthan. Chitosan has significant synergized the enhancements of xanthan gum in the release. Rheological behaviour of the selected formula containing chitosan (2%) and xanthan gum (1.5) had shear thinning in nature showing a decrease in viscosity at the increasing shear rates. The selected formula was stable 6 mo at 40˚C/75% RH and 4˚C. The formula found was yellow viscous creamy preparation with the smooth homogenous appearance. The pH and the drug release was also found to be stable under storage conditions.Conclusion: Piroxicam release can be improved by preparing emulgel which stable and have good rheologic properties.
In this research Bi2S3 thin films have been prepared on glass substrates using chemical spray pyrolysis method at substrate temperature (300oC) and molarity (0.015) mol. Structural and optical properties of the thin films above have been studied; XRD analysis demonstrated that the Bi2S3 films are polycrystalline with (031) orientation and with Orthorhombic structure. The optical properties were studied using the spectral of the absorbance and transmission of films in wavelength ranging (300-1100) nm. The study showed that the films have high transmission within the range of the visible spectrum. Also absorption coefficient, extinction coefficient and the optical energy gap (Eg) was calculated, found that the film have direct ener
... Show MoreHydrogen sulfide removal catalyst was prepared chemically by precipitation of zinc bicarbonate at a controlled pH. The physical and chemical catalyst characterization properties were investigated. The catalyst was tested for its activity in adsorption of H2S using a plant that generates the H2S from naphtha hydrodesulphurization and a unit for the adsorption of H2S. The results comparison between the prepared and commercial catalysts revealed that the chemical method can be used to prepare the catalyst with a very good activity.
It has observed that the hydrogen sulfide removal over zinc oxide catalyst follows first order reaction kinetics with activation energy of 19.26 kJ/mole and enthalpy and e
... Show MoreBackground: Implant stability is a mandatory factor for dental implant (DI) osseointegration and long-term success. The aim of this study was to evaluate the effect of implant length, diameter, and recipient jaw on the pre- and post-functional loading stability. Materials and methods: This study included 17 healthy patients with an age range of 24-61 years. Twenty-two DI were inserted into healed extraction sockets to replace missing tooth/ teeth in premolar and molar regions in upper and lower jaws. Implant stability was measured for each implant and was recorded as implant stability quotient (ISQ) immediately (ISQ0), and at 8 (ISQ8) and 12 (ISQ12) weeks postoperatively, as well as post-functional loading (ISQPFL). The pattern of implant
... Show MoreMembrane manufacturing system was operated using dry/wet phase inversion process. A sample of hollow fiber membrane was prepared using (17% wt PVC) polyvinyl chloride as membrane material and N, N Dimethylacetamide (DMAC) as solvent in the first run and the second run was made using (DMAC/Acetone) of ratio 3.4 w/w. Scanning electron microscope (SEM) was used to predict the structure and dimensions of hollow fiber membranes prepared. The ultrafiltration experiments were performed using soluble polymeric solute poly ethylene glycol (PEG) of molecular weight (20000 Dalton) 800 ppm solution 25 °C temperature and 1 bar pressure. The experimental results show that pure water permeation increased from 25.7 to 32.2 (L/m2.h.bar) by adding a
... Show MoreA metal-assisted chemical etching process employing p-type silicon wafers with varied etching durations is used to produce silicon nanowires. Silver nanoparticles prepared by chemical deposition are utilized as a catalyst in the formation of silicon nanowires. Images from field emission scanning electron microscopy confirmed that the diameter of SiNWs grows when the etching duration is increased. The photoelectrochemical cell's characteristics were investigated using p-type silicon nanowires as working electrodes. Linear sweep voltammetry (J-V) measurements on p-SiNWs confirmed that photocurrent density rose from 0.20 mA cm-2 to 0.92 mA cm-2 as the etching duration of prepared SiNWs increased from 15 to 30 min. The
... Show MoreThis study aimed to develop a stable nanosuspension of repaglinide and improve its dissolution, using the Nano-precipitation method, involving a different concentration of a stabilizer, different co-stabilizers and different solvents. Employment of a systemic approach to optimize the formulation parameters, including stabilizer concentration, solvent choice and co-stabilizer election. Soluplus® (SOL) was used as the primary stabilizer for this research, polyvinyl alcohol (PVA), poloxamer 188 (PXM 188), tween 80 (TW80), and polyvinyl pyrrolidine (PVP k30) were investigated as co-stabilizers to prevent particle agglomeration and ensure long-term stability. In addition to ethanol as a primary solvent, acetone and chloroform were used
... Show MoreHealth and environmental factors as well as operational difficulties are major challenges facing the development of an anaerobic digestion process. Some of these problems relate to the use of sludge collected from primary and secondary clarifier units in wastewater treatment plants for laboratory purposes.
The present study addresses the preparation of sludge for laboratory purposes by using a mixture that consists of the digested sludge, which is less pathogenic, compared to the collected sludge from the primary or secondary clarifier, and food wastes. The sludge has been tested experimentally for 19 and 32 days under mesophilic conditions. The results show a steady methane production rate from the anaerobic dig
... Show MoreThree ligands were prepared, spectroscopic method and elemental analysis verified their structures. The L1 and L2 ligands are flavylium salts while the third one L3 is a Flavon. The reactions between transition metal salts and the ligands have synthesized two groups of new metal complexes, one group contains L1, L3 coordinated with the metal ion. The other group contains L2, L3 and the metal. These complexes have been identified by available spectroscopic tools (UV-Visible and IR), the C.H.N results confirmed the proposed structures. The experimental data disclosed that the complexes were coordinated by 6the coordinate with mono-and bidentate ligands forming octahedral structure, in which L3 acts as monodentate and L1, L2 as bidentate ligan
... Show More