Background: The most common reason for re-making a maxillofacial prosthesis is the degradation of the mechanical properties of the silicone. Aim of this study: To assess some mechanical properties of VST-50F maxillofacial silicone reinforced with a composite of silicon dioxide nanoparticle and polyamide-6 microparticle before and after artificial aging. Material and Method: Preparing 240 samples tested for tear strength, tensile strength and elongation percentage, hardness, and roughness before and after aging. The Silicon dioxide was added in concentrations of 1% by weight and Polyamide-6 in the concentration of 0.25% and 0.5% by weight to the VST-50F RTV maxillofacial silicone. The one-way ANOVA and post hoc tests were used for inferential statistics. Results: The one-way ANOVA showed a highly significant difference between all tested groups. The effect of the addition of composite fillers showed an increase in tear strength, hardness, and surface roughness but a decrease in tensile and percentage of elongation. However, the effect of artificial aging showed increased in tear strength, Percentage of elongation, and surface roughness, but a decrease in tensile strength and hardness. Conclusion: Addition of composite of fillers into the silicone elastomer allowed enhancement of some mechanical properties. The composite of different types of filler reinforcement improves the anti-aging properties of silicone and maintain some of the mechanical properties to enhance the service life.
The V2O5 films were deposited on glass substrates which produce using "radio frequency (RF)"power supply and Argon gas technique. The optical properties were investigated by, UV spectroscopy at "radio frequency" (RF) power ranging from 75 - 150 Watt and gas pressure, (0.03, 0.05 and 0.007 Torr), and substrate temperature (359, 373,473 and 573) K. The UV-Visible analysis shows that the average transmittance of all films in the range 40-65 %. When the thickness has been increased the transhumance was decreased from (65-40) %. The values of energy band gap were lowered from (3.02-2.9 eV) with the increase of thickness the films in relation to an increase in power, The energy gap decreased (2.8 - 2.7) eV with an increase in the pressure and
... Show MoreBackground: The most widely used material for fabrication of denture base is poly methyl methacrylate, despite its popularity, the main problems associated with it as a denture base material are poor strength particularly under fatigue failure inside the patient mouth, impact failure outside the patient mouth, which are the main causes for fracture of denture, several studies was done to increase mechanical properties of denture base. The present study was conducted to evaluate and compare the effect of addition single walled carbon nanotubes in different concentrations to polymethyl methacrylate on some mechanical properties (surface hardness, surface roughness, impact strength and transverse strength). Materials and methods: Forty eight
... Show MoreIn this paper, three tool paths strategies; iso-planar, helical and adaptive have been implemented to investigates their effect on the mechanical properties of Brass 65-35 formed by single point incremental sheet metal forming process. To response this task, a fully digital integrated system from CAD modeling to finished part (CAD/CAM) for SPIF process has been developed in this paper.
The photo-micrographs shows an identical grain formation due to the plastic deformation of the incremental forming process, change in the grain shape and size was observed. It's found that the adaptive tool path play a significant role to increase the hardness of the formed specimen from (48 to 90 HV) and the grain texture of the formed specimen found a
PMMA (Poly methyl methacrylate) is considered one of the most commonly used materials in denture base fabrication due to its ideal properties. Although, a major problem with this resin is the frequent fractures due to heavy chewing forces which lead to early crack and fracture in clinical use. The addition of nanoparticles as filler performed in this study to enhance its selected mechanical properties. The Nano-additive effect investigated in normal circumstances and under a different temperature during water exposure. First, tests applied on the prepared samples at room temperature and then after exposure to water bath at (20, 40, 60) C° respectively. SEM, PSD, EDX were utilized for samples evaluation in this study. Flexural
... Show MoreIn this study, the mechanical properties of an epoxy and unidirectional woven carbon with fiberglass composite were experimentally investigated. When preparing the composite samples, American Society for Testing and Materials (ASTM)standard was used. Tensile, impact and flexural test were conducted to investigate the mechanical properties of the new produced epoxy Unidirectional Woven Carbon and Epoxy Fiberglass composites. The outcome showed that the strength of the produced samples increased with the increase in the number of unidirectional woven carbon layers added. Two methods were utilized: (1) woven carbon composite with glass fiber (2) woven carbon composite). The two methods of composite were compared with each other. The resul
... Show MoreBackground: Diabetes mellitus is a major risk factor for chronic periodontitis (CP) and hyperglycemia has an important role in the enhancement of the severity of the periodontitis. It has been reported that the progression of CP causes shifting of the balance between bone formation and resorption toward osteoclastic resorption, and this will lead to the release of collagenous bone breakdown products into the local tissues and the systemic circulation. Cross-linked N-telopeptide of type I collagen (NTx) is the amino-terminal peptides of type I collagen which is released during the process of bone resorption. This study was conducted to determine the effects of nonsurgical periodontal therapy on serum level of NTx in type 2 diabetic patients
... Show MoreBackground: This study aimed to compare the mechanical properties between four groups of newly fabricated combination wires according to their method of union, according to the gauges of wires and a comparison were made between them and their originals. Materials and method: A total of 60 stainless steel combination wires were fabricated , divided into four groups according to gauge of wires and their method of union, each of them with 15 samples, the groups were welded (0.016x0.022-0.016 and 0.016x0.022-0.018) and soldered (0.016x0.022-0.016 and 0.016x0.022-0.018), samples were made according to certain parameters which were : for the welded samples: length,weight, duration of pulsation and size of copper electrode tips used; for the sold
... Show MoreThe optical properties for the components CuIn(SexTe1-x)2 thin films with both values of selenium content (x) [0.4 and 0.6] are studied. The films have been prepared by the vacuum thermal evaporation method with thickness of (250±5nm) on glass substrates. From the transmittance and absorbance spectra within the range of wavelength (400-900)nm, we determined the forbidden optical energy gap (Egopt) and the constant (B). From the studyingthe relation between absorption coefficient (α) photon energy, we determined the tails width inside the energy gap.
The results showed that the optical transition is direct; we also found that the optical energy gap increases with annealing temperature and selenium content (x). However, the width of l