Two common iron oxide-bearing wastes—a drinking water treatment residual and a passive mine water treatment sludge (MWTS)—were utilised with and without modification as media in microcosm experiments to treat artificial benzene, toluene, ethylbenzene, and xylene (BTEX)-contaminated wastewater. In all cases, the removal of BTEX was observed over the 160-day experiments, with benzene being the most recalcitrant. The solubilisation of iron was observed, which, alongside the syntropic relationship between the methanogens and firmicutes, allowed several anaerobic processes to occur, including iron reduction in concert with the biodegradation of BTEX. Nitrogen sparging prior to microcosm establishment, compared to aeration, was seen to lead to the greater subsequent removal of BTEX, indicating that anaerobic conditions favoured removal. The rates of BTEX removal indicated that these iron oxide-bearing wastes, an abundant waste stream, may be an interesting candidate for cost-effective media for BTEX remediation in applications such as permeable reactive barriers.
In this study, Zinc oxide nanostructures were synthesized via a hydrothermal method by using zinc nitrate hexahydrate and sodium hydroxide as a precursor. Three different annealing temperatures were used to study their effect on ZnO NSs properties. The synthesized nanostructure was characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), Atomic force microscope (AFM), and Fourier Transform Infrared Spectroscopy (FTIR). Their optical properties were studied by using UV -visible spectroscopy. The XRD analysis confirms that all ZnO nanostructures have the hexagonal wurtzite structure with average crystallite size within the range of (30.59 - 34
... Show MoreIndium oxide In2O3 thin films fabricated using thermal evaporation of indium metal in vacuum on a glass substrate at 25oC using array mask, after deposition the indium films have been subjected to thermal oxidation at temperature 400 °C for 1h. The results of prepared Indium oxide reveal the oxidation method as a strong effect on the morphology and optical properties of the samples as fabricated. The band gap (Eg) of In2O3 films at 400 °C is 2.7 eV. Then, SEM and XRD measurements are also used to investigate the morphology and structure of the indium oxide In2O3 thin films. The antimicrobial activity of indium oxide In2O3 thin films was assessed against gram-negative bacterium using inhibition zone of bacteria which improved higher ina
... Show MoreAbstract
There has been a heated controversy over the role the financial policy plays and how sufficient it is in affording the financial burden. This burden is known as the operational current expenses which the governments of various countries mainly afford, despite the discrepancy in the government’s economic policy. After the deterioration and deficit in the state budget in all countries nowadays, it was necessary to find an appropri
... Show MoreThe coefficient of performance of a window type Air-Conditioner system can be improved if a reduction in the work of compressor can be achieved by a suitable technique. The present study investigates the effect of dispersing a low concentration of TiO2 nanoparticles in the mineral oil based lubricant, as well as on the overall performance of a window type Air-Conditioner system using R22 as the working fluid. An enhancement in the COP of the refrigeration system has been observed and the existence of an optimum volume fraction noticed, with low concentrations of nanoparticles suspended in the mineral oil. Results showed that the average compressor work reduced by 13.3%, which ultimately resulted in an increase of 11.99% in the COP due to
... Show MoreCurrent studies interested on the biosynthesis of zinc oxide nanoparticles (ZnO-NPs) using hot plants extracts of Allium sativum and characterization of them using: Atomic Force Microscopy (AFM), X-ray diffractions (XRD), Fourier Transform Infrared Spectroscopy (FT- IR), UV–visible spectral and Hot stage. The results found that all NPs are had nano-size. ZnO NPs was produced by four procedures using hot extract of Allium sativum. The average diameters were: 101.59 nm, 110.33 nm, 75.69 nm, 88.67 nm for first, second, third and fourth procedures respectively compared with 47.57 nm for standard NPs. The Roughness averages (Ra) were: 10.8 nm, 6.83 nm, 13.8 nm, 0.541 nm for first, second, third and fourth respectively. The Root mean square (Sq
... Show More