Background This study aimed to develop remineralizing calcium-phosphate (CaP) etchant pastes for enamel conditioning before bracket bonding and evaluate the bonding performance, failure pattern, and enamel surface integrity post bracket debonding in comparison with the conventional phosphoric acid (PA) etchant gel. Material and Methods Micro-sized monocalcium phosphate monohydrate and hydroxyapatite (micro- and nano-sized) powders were mixed with various phosphoric and nitric acid concentrations to develop eight acidic CaP pastes. Ninety extracted human premolars were randomly assigned into eight experimental and one control group (n=10). The developed pastes and control (commercial 37% PA-gel) were applied onto the enamel using the etch-and-rinse protocol before bonding metal brackets. Shear bond strength and adhesive remnant index (ARI) scores were evaluated after 24 hours water storage (24 h) and post 5000 thermocycling (TC). Field emission scanning electron microscopy (FE-SEM) was used to evaluate enamel damage after bracket debonding. Results The developed CaP pastes, excepting MNA1 and MPA1, resulted in significantly lower SBS values and ARI scores than 37% PA gel. Etching with 37% PA yielded roughened, cracked enamel surfaces with excessive retention of adhesive residue. In contrast, enamel treatment with the experimental pastes exhibited smooth, unblemished surfaces, with obvious CaP re-precipitation induced by mHPA2 and nHPA2 pastes and to a lesser extent by MPA2 paste. Conclusions Three newly developed CaP etchant pastes (MPA2, mHPA2, and nHPA2) can be promising alternative enamel conditioners that outperform conventional PA by generating adequate bracket bond strengths besides precipitating CaP crystals on the enamel. Moreover, these pastes maintained unblemished enamel surfaces with no or minimal adhesive residue after bracket removal.
In a hybrid cooling solar thermal systems , a solar collector is used to convert solar energy into heat energy in order to super heat the refrigerant leaving the compressor, and this process helps in the transformation of refrigerant state from gaseous state to the liquid state in upper two-thirds of the condenser instead of the lower two-thirds such as in the traditional air-conditioning systems and this will reduce the energy needed to run the process of cooling .In this research two systems with a capacity of 2 tons each were used, a hybrid air-conditioning system with an evacuated tubes solar collector and a traditional air-conditioning system . The refrigerant of each type was R22.The comparison was in the amou
... Show MoreBackground: The accuracy of fitness of any dental casting is imperative for the success of any prosthodontic treatment. From the time that dental casting was first introduced, efforts have been made to produce more accurate and better fitted castings with minimal marginal discrepancy. The aim of this in vitro study was to evaluate the effects of three different investing and burnout techniques on the vertical marginal discrepancies ofceramometalcopings invested with two types of phosphate- bonded investments. Materials and methods: Sixty wax patterns were fabricated on a standardized prepared brass die representing an upper central incisor by the aid of a custom-made split mold. Three different investing and burnout techniques were applied
... Show MoreThe study aims to use the European Excellence Model (EFQM) in assessing the institutional performance of the National Center for Administrative Development and Information Technology in order to determine the gap between the actual reality of the performance of the Center and the standards adopted in the model, in order to know the extent to which the Center seeks to achieve excellence in performance to improve the level of services provided and the adoption of methods Modern and contemporary management in the evaluation of its institutional performance.
The problem of the study was the absence of an institutional performance evaluation system at the centre whereby weaknesses (areas of improvement) and st
... Show MoreInterface bonding between asphalt layers has been a topic of international investigation over the last thirty years. In this condition, a number of researchers have made their own techniques and used them to examine the characteristics of pavement interfaces. It is obvious that test findings won't always be comparable to the lack of a globally standard methodology for interface bonding. Also, several kinds of research have shown that factors like temperature, loading conditions, materials, and others have an impact on surface qualities. This study aims to solve this problem by thoroughly investigating interface bond testing that might serve as a basis for a uniform strategy. First, a general explanation of how the bonding strength
... Show MoreInterface bonding between asphalt layers has been a topic of international investigation over the last thirty years. In this condition, a number of researchers have made their own techniques and used them to examine the characteristics of pavement interfaces. It is obvious that test findings won't always be comparable to the lack of a globally standard methodology for interface bonding. Also, several kinds of research have shown that factors like temperature, loading conditions, materials, and others have an impact on surface qualities. This study aims to solve this problem by thoroughly investigating interface bond testing that might serve as a basis for a uniform strategy. First, a general explanation of how
... Show MoreBackground: The aim of this in vitro study was to evaluate and compare the microleakage between Vertise Flow T M composite material and other conventional (Filtek Z250, riva light cure and SDR) composite materials when restoring CII mesial box only cavity at gingival margin through die penetration test Materials and methods: Forty maxillary first premolars were prepared with class II box design only cavities. Samples were divided into four groups of ten teeth according to material used: group I (FiltekZ250 only). Group II (SDR+FiltekZ250). Group III (Vertise Flow +FiltekZ250). Group IV (Riva light cure+ FiltekZ250). After 24 hrs. immersion in 2% in methylene blue, samples were sectioned and micro leakage was estimated. Results: None of the
... Show MoreBackground: Studying and investigating the transverse strength(Ts), impact strength(Is), hardness (Hr) and surface roughness(Ra) of conventional and modified autopolymerizing acrylic resin with different weight percentages of biopolymer kraftlignin, after curing in different water temperatures; 40°C and 80°C. Material and Methods: Standard acrylic specimens were fabricated according to ADA specification No.12 for transverse strength, ISO 179 was used for impact testing, Shore D for hardness and profilometerfor surface roughness. The material lignin first dispersed in the monomer, then the powder PMMA is immediately added. Ligninadded in different weight percentages. Then cured using pressure pot (Ivomet) in two temperatures;40°C a
... Show More