Steel corrosion in acidic environments is a critical industrial challenge, necessitating effective yet eco-friendly inhibitors. This study aims to address this problem by introducing a novel, green alternative: frankincense extract (FE). The distinctive contribution of this work lies in the comprehensive investigation of FE natural, sustainable, and economically viable resin as an effective corrosion inhibitor for carbon steel in 1 M HCl. The research employs an integrated methodology, including electrochemical techniques (potentiodynamic polarization (PDP) and electrochemical impedance spectroscopy (EIS)), adsorption isotherm modeling, surface analysis (FT-IR and FESEM/EDX), and density functional theory (DFT) calculations. Key results demonstrated that FE exhibited excellent inhibition performance, achieving a remarkable efficiency of 87.2% at a concentration of 16 g/L and 303 K. PDP analysis confirmed FE acts as a mixed-type inhibitor. EIS results corroborated this performance, showing 75.89% inhibition efficiency. Adsorption behavior adhered to the Langmuir isotherm, and thermodynamic parameters revealed a spontaneous and exothermic process indicative of mixed physisorption and chemisorption mechanisms. Kinetic studies further supported this by showing an increased activation energy barrier for corrosion in the presence of the inhibitor. Surface analysis confirmed the formation of a protective adsorbed film on the steel. Quantum chemical computations provided molecular-level insights, correlating the electronic structure of key FE constituents with their adsorption strength. The study establishes FE as a cost-effective, sustainable, and highly efficient green corrosion inhibitor, offering a viable solution for protecting carbon steel infrastructure in aggressive acidic media.
The aim of this research is to examine the relationship between entrepreneurial mindset and aspiration and small business performance Baghdad, Iraq. This study proposed a quantitative analysis in which entrepreneurial mindset and aspiration is a critical success factor of small business in Iraq. The method employed in the collection of data was by the means of self-administered questionnaire which was filled and completed by small business owners randomly selected from a sampling frame of registered small businesses. The questionnaire was adapted from the study of Davis, Halls & Mayer (2015) and Abdel-Maksoud, Asada & Nakagawa (2008) which was used to measure entrepreneurial mindset and aspiration using a ten items scale and small business
... Show MoreThe rapid increase in the number of older people with Alzheimer's disease (AD) and other forms of dementia represents one of the major challenges to the health and social care systems. Early detection of AD makes it possible for patients to access appropriate services and to benefit from new treatments and therapies, as and when they become available. The onset of AD starts many years before the clinical symptoms become clear. A biomarker that can measure the brain changes in this period would be useful for early diagnosis of AD. Potentially, the electroencephalogram (EEG) can play a valuable role in early detection of AD. Damage in the brain due to AD leads to changes in the information processing activity of the brain and the EEG which ca
... Show MoreIn the present study, MCM-41 was synthesis as a carrier for poorly drugs soluble in water, by the sol-gel technique. Textural and chemical characterizations of MCM-41 were carried out by X-ray diffraction (XRD), Fourier transform infrared (FTIR), scanning electron microscope (SEM), and thermal gravimetric analysis (TGA). The experimental results were analyzed mesoporous carriers MCM-41. With maximum drug loading efficiency in MCM-41 determined to be 90.74%. The NYS released was prudently studied in simulated body fluid (SBF) pH 7.4 and the results proved that the release of NYS from MCM-41 was (87.79%) after 18 hr. The data of NYS released was found to be submitted a Weibull model with a correlation coefficient of (0.995). The Historical
... Show MoreAbstract
Corrosion-fatigue occurs by the combined actions of cyclic loading and corrosive environment. The effect of shot peening on cumulative corrosion-fatigue life of 1100-H12 Al alloy was investigated. Before fatigue testing, specimens were submerged in 3.5%NaCl solution for 71 days. Constant fatigue tests were performed with and without corrosive environment. Cumulative corrosion-fatigue tests were also carried out in order to determine the fatigue life before and after shot peening. The constant fatigue life was significantly reduced due to corrosive environment and the endurance fatigue limit was reduced by 13% compared with dry fatigue. In case of shot peening the cumul
... Show Moreγ-Al2O3–NPs were synthesized by a green synthesis process based on Boswellia carterii resin extract and aluminum sulphate in an alkaline medium. Boswellia carterii resin extract is a significant reducing and stabilizing agent for synthesizing γ-Al2O3–NPs.Several techniques, including Fourier–transform infrared (FT-IR), UV–visible spectroscopy, x-ray diffraction, electron microscopy (XRD), energy dispersive x-ray (EDX), scanning electron microscopy (SEM), Transmission electron microscopy (TEM), and atomic force microscopy (AFM), were utilized to investigate the final product. XRD and SEM confirmed a plate-like crystalline structure with an average size of 17.5 nm. FT-IR analysis identified aluminum oxide stretching vibrations (655,
... Show MoreIn this paper, the behavior of spliced steel girders under static loading is investigated. A group of seven steel I-girders were tested experimentally. Two concentrated loads were applied to each specimen at third points and the load was increased incrementally up to the yield of the specimen. Two types of splices were considered; the bearing type and the friction-grip type splices. For comparison, an analytical study was made for the tested girders in which the finite element analysis program (Abaqus) was used for analysis. It was found that the maximum test load for spliced girders with bearing type splices was in the range of (34%) to (67%) of the maximum test load for the reference girder. For girders spliced by using friction-grip t
... Show Morehe paper presents the results of exposure of normal concrete to high temperatures (400 and 700°C). In addition to the exposure of steel reinforcement bar Ø 12 mm, where two types of steel reinforcement burning situations were performed. Directly exposed to high temperatures (400 and 700°C) and others were covered by concrete layer (15 mm). From the experimental results of fire exposure for 1 hour of 400 and 700°C and gradually cooled, it was found that the residual average percentage of compressive strength of concrete was 85.3 and 41.4%, while the residual average percentage of modulus of elasticity of concrete was 75 and 48%, respectively. The residual average percentage of yielding tensile stress (Ø 12 mm) after burning and cooling
... Show MoreCorrosion resistance of metals is one of the most important topics for researchers. In this work, epoxy-TiO2 nanocomposite has been developed for protection of 6061AL alloy. The dip-coating technique used to deposit the coating on 6061 Al alloy substrate. Different concentrations of TiO2 NPs (1,3,5 )Wt% have been used to study the corrosion behavior in 3.5% NaCl medium. Also, 200,150 and 100 mm/min dipping speeds have been employed for 1%wt TiO2 to show their effects on coating layer and corrosion rate. Characterization of coated surfaces were investigated by AFM, FESEM andEDS,while theelectrochemical measurementswas using to evaluate protective nature of the coating. The results have shown that the corrosion rate has decreased with
... Show More